SWD6006 elastic waterproof coating material takes one-component environmental-friendly water-borne polymer resin as main raw material, and refined through scientific production process. The coating is compact, has strong adhesion with various kinds of substrates. It has excellent sealing and impermeability, good hiding power, excellent anti-aging performance, it will not peel off or powder after long-term outdoor use. It has excellent waterproof protection on building surfaces, which has been widely used in Europe and the United States.


Product Detail

Product Tags

Features and benefits

The film is compact and has good adhesion force, integral forming waterproof system

Excellent anti-aging performance, long-term outdoor use will not fall off, or powder or color-changing, it will extend the service life.

Excellent flexibility in low temperature, -40 Centigrade

Anticorrosion and chemical resistance

Excellent waterproof, anti-mildew performance

Water based coating, environmentally friendly, toxic free, safe material.

Easy to apply, it is a replacement product to tar-based polyurethane waterproof coating

Product application scope

Concrete roof, steel roof, kitchen bathroom floor, bathroom, reservoir, basement, waterproof membrane and old roof SBS waterproof and renovation works (such as asphalt, PVC, SBS, polyurethane and other base) 

Product information

Item Results
Appearance White or gray
Glossy Matte
specific gravity (g/cm3) 1.12
Viscosity (cps )@20℃ 420
Solid content (%) 71%±2%
surface dry time (h) Summer: 1-2h, winter: 2-4h
theoretical coverage 0.17kg/m2(thickness 100um)

Physical property

Item Test standard Results
Hiding power (white or light color)/(g/m²) JG/T235-2008 ≤150
Dry time/h JG/T172-2005 Surface dry time≤2; solid dry time≤24
Adhesion (cross cut method) / grade JG/T172-2005 ≤1
Impermeability JG/T172-2005 0.3MPa/30min, Impermeable
Impact resistance /cm JG/T172-2005 ≥30
Tensile strength JG/T172-2005 ≥1.7Mpa
Elongation rate JG/T172-2005 ≥200%
Tear resistance,≥kN/m   JG/T172-2005 35
Temperature resistance of coating (5 cycles) JG/T172-2005 Normal 

Corrosion resistance property

Acid resistance c(5%H2SO4 JG/T172-2005 168 h, normal
Salt spray resistance JG/T172-2005 1000 h , no peel off, no peel off
Artificial accelerated anti-aging  (1000h) Tensile strength retention, %         85
Elongation rate, %             ≥150

Application environment

Environment temperature: 5-35℃

Humidity: ≤85%

Application instructions

Recommended dft (1layer) 200-300um
Recoating time (25℃) Min:4h, Max: 28h
Recommended application method Roller, brush

Application tips

The surface should be clean, without any oil, rust or dusts.

The remaining material is not allowed to pour back to the original drums.

It is water-based coating, don’t add other organic solvents or other coatings in it.

Product curing time

Substrate temperature surface dry time foot traffic solid dry
25℃ 40 min 12h 7d

Product storage and shelf life

Storage temperature:+5-35°C

Shelf life: 12 months (unsealed)

Keep the products seal well, store in cool and ventilated place, avoid direct sunshine exposure.

Package: 20kg/drum

Product health and safety information

For information and advice on the safe handling, storage and disposal of chemical products, users shall refer to the latest Material Safety Data Sheet containing physical, ecological, toxicological and other safety related data.

Integrity declaration

SWD guarantee all technical data stated in this sheet are based on laboratory tests. Actual testing methods may vary due to different circumstances. Therefore please test and verify its applicability. SWD does not take any other responsibilities except the product quality and reserve the right of any modifications on the listed data without prior notice.


  • Previous:
  • Next:

  • Write your message here and send it to us